Thermochemical Properties
Propellant | Flame Temperature | Specific Energy | Heat of Explosion | Ratio of Specific heats | Covolume | Density | |||
---|---|---|---|---|---|---|---|---|---|
(K) | (°C) | (°F) | (J/g) | (J/g) | (Cal/g) | (Cp/Cv) | (cm³/g) | (g/cc) | |
S265 | 3 062 | 2 789 | 5 052 | 1 030 | 3 667 | 876 | 1.237 | 1.003 | 1.55 |